Calculate Recoveries with 2 or 3 Product Formulas

Two Product Recovery Formula

Here is the formula you need to calculate Metal Recoveries using Assays only.  You have two products/concentrates.  This will save you time in your metallurgy accounting calculations.  Some call the same formula the two (2) product other the three (3) product formula. Frequently, a concentrator will mill a complex ore requiring the production of two separate […]