Effect of Cyanide on Depression of Sulphide Minerals

effect of NaCN cyanide on sulphide depression in flotation

At the dosage of collector (not shown but relatively low), it is indicating galena will not float above pH 10.4, and it is not affected by NaCN. What you have to be careful about is that these lines all move if you increase or decrease the collector dosage. For example, you can get pyrite to […]