Agitated Leaching Circuit Operation

Leaching Circuit

Ground slurry from the trash screen enters this EXAMPLE Agitated Leach circuit at a rate of 35.5 cubic meters per hour, and 45% solids. The slurry passes through each of the four tanks, and should remain in each tank for a period of approximately 12 hours. Each tank is 8 meters in diameter by 8.5 […]