Gold in Deep Gravel Deposit

Both in Australia and California, besides the superficial placer deposits situated in or near the existing rivers, which in the deep canons of the Klamath and other rivers in the extreme north of California attain a thickness of 250 feet, there exist auriferous gravels which bear no apparent relation to the present drainage of the […]
Placer Mining Cost
In work on shallow placer deposits by individuals the results differ greatly, both according to the strength and skill of the worker and to the contents of the gravel. Under the best conditions of climate a strong, well-nourished, American digger may be able to raise by the shovel from 10 to 12 cubic yards of […]
Placer Gold Mining Methods

The gold deposits grouped together under the name of “ placers ” comprise sands, gravels, or any loosely coherent or non-coherent alluvial beds containing gold. They have accumulated owing to the action of running water, in the beds of rivers, or on the adjoining inundation plains, or on sea beaches. They fall naturally into two […]