Assaying

Assaying for ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, gold is performed by fire assay. This ancient form of quantitative chemical analysis by which metals are separated and determined in ores and metallurgical products with the aid of heat and dry reagents. At present, this technique is used principally to preconcentrate the noble metals from … Read more