Rotary Kiln Maintenance

Rotary Kiln Alignment The continuity of operation of a lime sludge kiln requires strict maintenance control. The rotary kiln is among the largest type of moving machines made and is subjected to extreme temperatures, power failures, atmospheric conditions, varying loads, and other operating conditions which affect its wear and alignment. It should be erected under […]
Rotary Lime Kiln Operation

Precipitated calcium carbonate, commonly called lime sludge or lime mud, is produced when sulphate green liquor is causticized with lime. For many years this lime sludge was considered a waste product and was dumped into rivers or waste ponds, or used for fill around the plants. Large quantities of new lime were purchased from commercial […]
Clinker Cooler

The Air-Quenching shaking grate Clinker Cooler was developed more than 20 years ago as an improved heat recuperating cooler for use with rotary kilns. It was designed to air quench and cool large quantities of hot clinker rapidly, and to recover and return to the kiln a major portion of the heat from the clinker. […]