Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

Hydrometallurgy: Leaching in Heap, Vat, CIL, CIP, Merrill–Crowe, SX Solvent Extraction

  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Hydrometallurgy.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Which chemical can i use to treat zinc in vat leaching? (1 reply)

S
Janka
2 months ago
Janka 2 months ago

how can i treat zinc in vat leaching?

J
Jorge
2 months ago
Jorge 2 months ago

First and foremost, it is necessary to perform some tests in the met lab. you should evaluate the effect of sulphuric acid on zinc dissolution. Some time ago, I performed some tests, the main zinc mineral was willemite, and the presence of smithsonite and hydrozincite was not not important. The particle size is other parameter to evaluate (e.g. 1/2", 3/4", 1"). Also, it is necessary to perform some tests to determine the optimum sulphuric acid strength (e.g. 5g/l, 10g/l, 15g/l).

During the testing program, some sample of pregnant solution must be taken to estimate the zinc extraction.