Corrosion During Ore Grinding

Ore grinding is a major cost operation for the mineral processing industry. The U.S. mining industry consumes more than 400,000 st of grinding rods, balls, and mill liners in wet grinding operations at an annual cost of $300 million a significant portion of the milling cost. A section of a commercial ore grinding operation is […]

Mine Waste Tailings Beaching

The Bureau of Mines surveyed waste disposal sites at 18 metal and non-metal mines and conducted laboratory and full-scale field tests to determine the effects of tailings deposition techniques on physical properties of tailings pond beaches. Survey data included measurements of beach slopes, descriptions of deposition techniques, and measurements of beach physical properties taken at […]

Modelling Solvent Extraction of Copper in Ammoniacal Systems

A mathematical modeling method was developed by the Bureau of Mines for the prediction of the principal equilibrium species in the solvent extraction of copper. The use of models for predicting the amount of metal extracted can reduce the amount of experimental work required to characterize a system for purposes such as optimization studies. Models […]

Column Flotation and Bubble Generation

As part of its research program on column flotation, we performed studies on (1) column flotation amenability and comparison with conventional flotation results for over 15 mineral systems, (2) alternative methods for improving column bubble generation systems, (3) mineral behavior within a column, and (4) the effect of changes in column operating parameters on flotation […]

Recovering Lithium from Clays

Preliminary Lithium Extraction Tests: In the preliminary McDermitt clay studies, several lithium extraction methods were investigated. Water disaggregation, hydrothermal treatment, acid leach, alkaline roast-water leach, sulfate roast-water leach, and chloride roast-water leach were techniques used in the treatment of both McDermitt A and B clays. Only the higher grade McDermitt B clay was treated by the […]

Electrowinning Tankhouses Air Quality

Electrowinning is an electrochemical operation employing an anode and cathode immersed in an electrolytic solution containing sulfuric acid and aqueous copper sulfate. When direct electrical current passes between the cathode and anode through the electrolyte, very pure metallic copper is deposited on the surface of the cathode. The process is conducted commercially in electrolytic cells […]

Re-agglomeration in Fine Grinding of Coal

There is a growing interest in the use of fine grinding to produce ultrafine particles for applications such as direct firing of micronized coal. It has been long known that the difficulty of grinding increases dramatically with the fineness of the desired product. To some extent this is a direct consequence of the decrease in […]

Reduce Ball Mill Wear by Cathodic Protection

The present work was undertaken to develop a method to cathodically protect a ball mill to reduce materials loss from mill liners. The essential science of “Cathodic Protection” is to apply a sufficiently negative potential to a metal in a corrosive environment such that the anodic corrosion rate is reduced to a negligibly small or […]

Iodide Pressure Oxidation Gold Leaching – Autoclave

The pressure oxidation process is especially suitable for the sulfide type of refractory ores. It includes two stages of operation. First, the refractory ore is subjected to an autoclave oxidation. At elevated temperatures usually above 180°C and in acidic or alkaline medium and pressurized oxygen, sulfide minerals are oxidized for a period of 1-2 hours. […]