Colemanite Clay Flotation

Floatability of colemanite was determined using a 150-ml column cell (25 x 220 mm) with a fine fritt and magnetic stirrer. One gram of sample was conditioned in 150 ml of a solution containing SDS for 10 min. and floated for one min. using nitrogen gas at a flow rate of 50 cm³/min. The microflotation […]

Acid Activated Montmorillonites Uses

Non-swelling calcium montmorillonite is mined from bentonite deposits and treated to produced acid-activated powders and granules for use as separation products and catalysts. In particular, acid-activated montmorillonites are used as sorbents for removing impurities from fats and oils, as catalysts for mineral oil processing and for a number of other applications. These smectite group minerals […]

Column Flotation Cell Baffles

The increased use of flotation columns is due to their superior separation efficiency compared to conventional flotation. This increased efficiency can be attributed to: The countercurrent movement of slurry and air bubbles increases the probability of bubble / particle attachment. This is accomplished by larger aerated volume of the cell, longer concentration gradient between froth […]

First Order Flotation Rate Equation

Many investigators showed that mineral flotation can be described as a first-order process (Sutherland, 1948; Tomlison and Fleming, 1963). In this case, the rate of flotation can be represented by: dN/dt = -kN……………………………………………………(1) where N is the number of floatable (or hydrophobic) particles present in a flotation cell and k is the rate constant. It […]

Palladium Leaching in Ammonia

Recently, a number of techniques of recovering Palladium have been developed. For example, leaching of platinum group metals from spent automobile catalytic converters using halogen salt with oxygen was developed. Ammonia is an inexpensive lixiviant used in leaching precious metals such as silver and gold. Since palladium has some similar chemical properties to silver, it […]

Chalcopyrite Leaching by Iodine

Chalcopyrite is the most abundant mineral of copper sulfide minerals and the major source of copper. Numerous leaching processes, such as ammoniacal systems, acid sulfate systems, chloride systems, and nitrate systems, have been introduced and investigated. In oxygenated ammoniacal solutions, chalcopyrite dissolves according to the following reaction: CuFeS2 + 4NH3 + 17/4 O2 + 2OH- […]

Types of Pressure Oxidation Autoclave Lining

As shown in Figure 1, there are other accessory vessels (splash and flash towers) in the autoclave circuits, that are also brickwork lined. The linings used to date, other than small test sections, have all been acid-resistant fireclay bricks, bonded with alkali silicate mortar, PbO-based mortar, and/or vinyl ester mortar, but mainly alkali silicate mortar. […]

Coal Washing Plant

The calculation of the performance of coal washing units that are in common use is not difficult and the principles of making such calculations have been known for many years. The flowsheets to be simulated consist primarily of coal washing units each with a target specific gravity of separation specified for each washing unit. The […]

Flotation of Low Quality Coal

To understand interactions between physical and chemical variables, a synthesis rather than an analytical approach is needed. In analytical approach, sub-processes of a system are isolated to determine the cause and effect relationships between performance of the sub-process and the system variables, whereas in synthesis approach a global view is taken to identify various interactions. […]

Hypochlorite Leaching of Gold Ore

The reactions between gold and hypochlorite leach solutions containing hydrochloric acid and sodium chloride are demonstrated below: 4Au + 16NaOCl + 10H2O → 4HAuCl4 + 16NaOH + 5O2……………………………………(1) 4HAuCl4 + 4NaCl → 4NaAuCl4 + 4HCl…………………………………………(2) 16NaOH + 16HCl → 16NaCl + 16H2O…………………………………………(3) Overall reaction of equations (1), (2) and (3) can be summarized as follows: 4Au + 16NaOCl […]