Laboratory Zadra Electrolytic Cell

A ZADRA electrolytic cell adapted to strip gold from sulfide solutions thereof which comprises a cathode assembly having a vertical metallic pipe adapted to deliver gold-bearing solution to the cell and to serve as a negative bus bar for delivering electric current to said cell, said pipe being axially positioned in said cell and being […]

Placer Mining Equipment

Specific placer mining equipment is needed for each of the methods which can be classified according to the several methods of excavating and transporting the gravel, or they may be designated to correspond with the various ways of saving the gold. The actual moving of the gravel from place is always the principal concern of […]

Sampling Placer Deposits by Drilling

The sampling of placer deposits by drilling or, more precisely, drive-pipe sampling, is discussed in detail by Janin. He states that the Keystone no. 3 traction machine is used generally in California. The usual casing is 6 inches inside diameter and 3/8 inch thick, in 5- to 7-foot sections. Drilling without casing is not good […]

Placer Gold Prospecting Equipment

The outfit to be taken on a prospecting trip depends upon the mode of transportation, the work contemplated, and the funds available. Enough equipment should be taken, but unnecessary articles make extra work. When a more or less permanent camp is established, added equipment for personal comfort and efficiency can be obtained. Usually a cabin […]

Gold Placer Sampling and Estimation

Failure to sample and estimate properly the available yardage of placer deposits has resulted in a tremendous waste of money and effort. A large proportion of all placer operations has failed because the gold in the gravel was insufficient to repay the cost of even the most efficient mining, not to mention the return of […]

Minerals Associated or Found in Gold Placer Gold

Associated Minerals: Placer gold invariably is accompanied by other heavy minerals, which comprise the black, white, or yellow concentrates found in the sluice box when cleaning up. Table 3 lists these minerals roughly in the order of their commonness. Some of the characteristics noted under Remarks apply chiefly to the minerals as they are found in […]

Zirconium Crucibles

Zirconium crucibles are rapidly becoming a standard piece of equipment, particularly in laboratories where fusions using strongly alkaline fluxes are common. This Center has found no better material to use for the thousands of sodium peroxide fusions that are done here every year. Zirconium crucibles usually arrive from their suppliers in a polished, silvery state. […]

Acid Digestion of Ferrochrome Metal

At times it may be necessary or desirable to dissolve a ferrochrome sample in acid rather than fusing it in sodium peroxide. Acid digestion methods are slow, but require little in the way of attention. Two alternative methods are described here. The A method is the basic method to use for most ferrochrome samples. The […]

Manganese in Chromite, and Ferrochrome

Manganese commonly occurs in mineral chromite as an impurity, and the amount can range from trace quantities to a few percent. In ferrochrome smelting operations, the manganese should find its way into the slag rather than the metal. Data from these analyses have most often been used to trace the partitioning of the manganese through […]

Gravimetric Silica in Chromite and Ferrochrome Slag

Silica is present in chromite ores as a basic silicate. In characterization and beneficiation studies performed on chromites at this Center, the chromium-silica ratio determines the purity of the gangue material being analyzed. Accurate characterization of the original ore material and the further feasibility of smelting to ferrochrome are identified by using this ratio. The […]