Bond Impact Crushing Work Index -Procedure

Sizing a crusher can be done reliably calculated thanks to the Impact/Crushing Work Index and the testwork research done by Fred Chester Bond and his 1952 paper. According to Bond’s Third Theory of Comminution, the work/energy input is proportional to the new crack tip length created during particle breakage and equivalent to the work represented by […]
Fine Gravity Gold

Here are images of gold ores rich in sulfides including arsenopyrite. Some of the ore types in these photos: https://en.wikipedia.org/wiki/Breccia https://en.wikipedia.org/wiki/Hornfels https://www.merriam-webster.com/dictionary/intrusion https://en.wikipedia.org/wiki/Limestone https://en.wikipedia.org/wiki/Volcanogenic_massive_sulfide_ore_deposit https://tinyurl.com/qcazwv8
Disclaimer
Nothing contained in the calculators, equations or other information on this website constitutes advice. Access to the calculators, equations and other information is donated for academic and research purposes only, and must only be used by qualified comminution/process engineers. Comminution/Process engineers considering the calculators, equations and other information must use their own professional judgement, knowledge […]
Let Us Not Forget
Mining & Mineral Processing Pumps
The use of Asbestos Free Materials in Static Sealing on Pumps Thunder Horse Injection Pump Toward Reduced Pump Operating Costs Part 2 Avoiding Premature Failures Toward Reduced Pump Operating Costs Part 3 Minimizing the Effects of Wear and Optimizing Pump Efficiency Toward Reduced Pump Operating Costs Turbomachinery Laboratory (2) Turbomachinery Laboratory (3) Turbomachinery Laboratory Tutorial […]
Mineral Processing Laboratories

Finding a good and the right mineral processing laboratory and have your testing filled properly is important. Most metallurgical laboratories now are actually specialized. They will claim to “do-it-all” while what they can actually do truly depends on who their current staff is. You have hear the cliché on people are our greatest asset? Well, it […]
Sampling a Conveyor Belt

To sample a FINE free-falling stream (Sampling a Conveyor Belt with a cross-belt cutter) as depicted, a sampling cup shall be used with the minimum dimensions as given in figure below. In addition, the length of the cup should be at least three times the width of the falling stream to be sampled and the […]
Laboratory Methods of Sample Preparation

Sample preparation method and Laboratory sampling procedures involve either: Coning and Quartering; or Riffling Method. Coning and Quartering for sample preparation techniques/method The method which is used for sampling large quantities of material say 20kg, consists of pouring or forming the material into a conical heap upon a solid surface (e.g. a steel plate) and relying on […]
Bond Work Index Procedure and Method

This Grindability Test or Bond Ball Mill Work Index Procedure is used to determine the Bond Work Index of minus six mesh or finer feed ore samples. These equation application methods are used to process <1/2″ ore samples in a Ball Mill using a standard ball charge. Below describes in general terms the Bond Work Index […]