The 911MPEFC250 is a Fine Jaw Crusher for pre-crushing of extremely hard up to brittle materials down to < 2mm in one step:
- End fineness 90% < 2mm
- Very Powerful
- Infinitely, reproducible gap adjustment
- Easily change of jaw plates and side liner
- Various infeed hopper: removable, with safety guard, batch loader and metering
- External control by Start/Stop
- Contamination free grinding
Superior Jaw Crusher engineered for pre-crushing of extremely hard up to brittle materials designed for batchwise and continuous pre-crushing of middle hard, hard brittle and tough materials for the following fine grinding.
Principle of operation
The 911MPEFC250 Jaw Crusher is used by laboratories and processing companies to crush solid materials such as rocks or soil and ores. The material to be processed falls into the crushing chamber of the LMC Crusher via a guide chute and is crushed by crushing action of a static and a dynamic jaw plate until it passes the preselected gap of the crusher.
Principle of operation for fine-crushing
Unlike conventional jaw crusher, the movable crushing jaw is guided in this jaw breakers in an oscillating motion. As a result the crushing gap
remains in the downward direction in the adjusted size and the product is crushed in a single step in this fineness.
Simple Cleaning and Operation
The 911MPEFC250 Fine Jaw Crusher has a 5″ x 10″ jaw cavity opening suitable for up to 180 Kilos/hr of material either batchwise or continuously. Moveable and fixed jaw plate as well as the side liner can be easily replaced.
Gap Adjustment
The requested gap setting can be adjusted comfortably and reproducibly.
Benefits and Advantages
- Improved power by 7500 Watts (3 phase – 10 HP) Motor
- Optimal grinding results by oscillating grinding movement
- Adjustable gap adjustment
- CE certified
- Removable indeed hopper, with safety guard or batch loader
- Base
- Spacious collector
- External control by Start/Stop
- P90 < 2 mm
- Contamination free grinding because of 4 different grinding tools*
- Easy exchange of jaw plates and side liners
Applications
- Minerals / Ores / Slags
- Cement / Cement Clinker / Concrete
- Glass / Ceramics / Corundum

- Soil Samples / Sludges
- Coal / Coke / Drill Core
- Industrial Waste
Specifications
| Maximum Feed Size | <110mm |
| End fineness | <2mm |
| Approximate Mass | 1000 Kg |
| Throughput | 180 Kg/h |
| Dust extraction points | 2 |
| Dust Extraction flow | 225L/sec. |
| Gap adjustment | Stepless |
| Electr. requirements (3-Phase) | 10 HP |

Jaw Crusher Liners & Cheek Plates
Jaw Plates / Side Liner Available in:
• Hardened steel
• Manganese steel
• Heavy metal free steel
• Stainless steel
Extremely robust crushing chamber:
• Jaw plates clamped from below by T-clamps
• Side Liner 12mm thickness
• Reinforced bearings
![]() | ![]() |
Complete Sample Preparation Station (Option)
Example Jaw Crusher Product

![]() | ![]() |