Drying Coal by Microwave
Fundamental problems exist with the drying of fine coal. The moisture content of fine coal after mechanical dewatering is often too high to allow the
Fundamental problems exist with the drying of fine coal. The moisture content of fine coal after mechanical dewatering is often too high to allow the

Development of the Hydrostatic Bearing Mechanism evolved from the caisson thickener design. Conventional thickener mechanisms are driven by gearing which rides on ball or roller
Figure 125, A and B shows typical arrangements using floating gold washing and gold-saving plants (“boats”). Figure 125, C, is a plan of an operation
Hydraulicking: In hydraulic mining a stream of water under high head is employed to break down the bank and excavate the gravel and to sweep it
Phosphatic clay waste is one of the principal waste products resulting from the mining and benefication of Florida phosphate ore. This waste material, which is

Marked ball wear testing described in a 1948 paper by Norman is an invaluable test method to measure relative and/or absolute wear rates of balls

Flameless AAS provides a means to increase flame AAS sensitivity, by up to 200 times. Interferences from aqueous leachates and digestates are so great, however,

Gold values in the surveyed sulfide-poor rock units proved to be generally even lower than those in sulfidic sandstone. As a further check on this

Enhanced gravity separation devices (centrifuges) have been patented for over a century but were impractical until recently. The physical laws behind the concept were well
A number of compressive tests were conducted on iron ore pellets obtained from the Samarco pelletizing plant located at Ponta Ubu, Brazil. These pellets are