Paste Backfills Types

The basic rule for a material to have paste fill flow properties is that it has at least 15 wt% of its particles finer than

Read More »

Shaft Sinking and Ramp Excavation

Mine planners and engineers are often faced with the decision of choosing which method of underground access is best suited for their particular requirement. Underground

Read More »

Titanium Mineralogy

The study of minero-petrographical characteristics and the subsequent textural and structural characterization of an ore mineral represents the first step of each industrial processing whose

Read More »

Grinding Circuit Expansion

Increasing ore hardness led to a gradual reduction of mill throughput rates. This, combined with declining head grades and low gold price, prompted a review

Read More »