LIX 64N
LIX 64N Reagent is a water insoluble mixture of substituted oximes, which form water insoluble complexes with metallic cations, principally copper. Chemical Reactions LIX 64N
LIX 64N Reagent is a water insoluble mixture of substituted oximes, which form water insoluble complexes with metallic cations, principally copper. Chemical Reactions LIX 64N

The ores of copper are usually associated with minerals containing arsenic, antimony and bismuth. Whatever the means adopted for extracting the copper, these metals are

The metallurgy of ores of titanium, titaniferous iron-ores (that is, iron-ores containing a notable amount of titanic acid, TiO2, say not less than 5 per
As this district is so far distant from the other mining centres and its mode of approach so circuitous, I am afraid that many residents
Methods of Crushing Stone without a Crusher Up to the date of the invention of the Stone Crusher, stone for road-metal was broken by hand,
The treatment of slimes has of late years been, the chief difficulty in connection with cyanide work, in which much time and money has been
Mixer Settler The Mixer-Settlers are of the pump-mixer type in which the Mixer Impellers, in addition to mixing the process liquors, also provide the pumping
It is often necessary to calculate the size of a mine hoisting system required to raise a given quantity of material, either as a preliminary
The presence of small amounts of tellurium in certain kinds of copper, and its exceptionally deleterious influence in producing red-shortness of this metal, led the
Petroleum The occurrence of petroleum in the Redington quicksilver-mine, New Idria, California, is reported by Luther Wagoner. He says: ‘‘ Mineral-oil occurs in considerable