Laboratory Procedures

Scorification Assay

As stated above, the Scorification Assay process is especially applicable to (a) complex ores, (b) very rich ores, (c) ores which are mainly valuable for

Read More »
ball-tube-and-rod-mills-dimensional-equation
Ball Mills

Grinding Process

In the previous chapter, the various “laws” of comminution which have been propounded have been studied in relation to the physical process of size reduction