The extraction and recovery process of vanadium as a by-product from the tailings of a uranium processing plant poses many problems. In this study vanadium is recovered

Solvent extraction, the process of extracting a specific metal valve from a solution to concentrate and purify that metal is a multistage process involving liquid

The flowsheet below Explains the Extraction of Tin Ore as shown by a study adapted to the concentration of a lode tin deposit. Cassiterite (SnO2)