Troughing Idlers
Feeders and Conveyors

Troughing Idlers

To start with the idlers, let’s look at the ones that carry the load first. They are called troughing idlers.   This type of idler

Read More »

Feeder Safety

Feeders can be dangerous, so lets talk feeder safety a bit.  All walkways and work areas should be kept clear for easy access and exits,

Read More »
slot feeder
Feeders and Conveyors

Slot Feeder

The slot feeder on the other hand is slightly different, all three types of feeders draw the ore from a fine ore storage area, usually

Read More »
Gate Feeder
Feeders and Conveyors

Fine Ore Feeders

This section is about the feeders that control the fine ore. This is the ore that has already been through the crushing stage of concentration.

Read More »
Sliding gate feeder
Feeders and Conveyors

Sliding Gate Feeder

The sliding gate feeder is used for the smaller ore sizes, in some applications it will even be used in our next group of feeders

Read More »
Vibratory Feeder
Feeders and Conveyors

Vibratory Feeders

Vibratory Feeders do not like wet ore much either but it is the next feeder type on my list. How this one works is quite

Read More »
Pan Feeder
Feeders and Conveyors

Pan Feeders

The next feeder on the list is the PAN FEEDER, this one may also be called the reciprocating feeder and it works like this. The

Read More »
Ross Feeder
Feeders and Conveyors

Ross Chain Feeders

A feeder that uses chains to regulate the ore flow in a different manner is the ROSS Chain FEEDER. This feeder uses a series of

Read More »