Vapor Pressure of Silver
The purpose of this study was to measure the vapor pressure of silver as the first step in the determination of activities in silver alloys

The purpose of this study was to measure the vapor pressure of silver as the first step in the determination of activities in silver alloys

G. Kuczynski and B. H. Alexander—This paper represents a most noteworthy attempt to evaluate experimentally the surface tension of a solid metal. Because of the

Mixers are being applied with increasing frequency to problems in the metallurgical industries. The increase represents in part the modernization of mechanical equipment used through

Callow-Type flotation cells, with various modifications, have been employed at the Hayden concentrator since 1917. Other flotation machines, such as matless-air and mechanically agitated types,

The behavior of collectors at the mineral-solution interfaces is usually explained in terms of an ionic adsorption process. Through the distribution of collector ions between

Separating a mixture of particle sizes of material suspended in a liquid medium is by no means an exact science. Selecting machines for individual classifying

The problems encountered in efforts to explain the behavior of limestones, dolomites, and related rocks as concrete aggregate lie on the frontiers between the ignorance

Conveyors were first used underground at Miami Copper Co., in the latter part of 1947. At that time some of the stoping area was too

The part that acceleration plays in starting a belt conveyor and its effect on belt conveyor design are well understood in a general way. Its

The heavy postwar demand for Portland Cement has created shortages that are gradually being overcome by increases in plant capacity. In the postwar period, the