An electronics recycler’s favorite, the RapidFire Pro-L offers the ultimate combination of portability, function, and performance demanded by professional artists, at a fraction of the cost of comparative products.

The RapidFire L is the ideal solution for jewelry, metal clay, and ceramic firing and comes complete with a digital control panel, embedded heating element, 6″ x 5″ x 6″ firing chamber, 1500 Watts of power, and wide opening door. And at just 12 lbs, it’s light enough to take with you on the go. RapidFire kilns are also available with programmable ramping controllers.
The RapidFire kilns are designed to rapidly heat to 2200 F (1205 C) for jewelry, metal clays (PMC), glass fusing, glaze testing and ceramics.
Art Clays, PMC, Glass Clays, Glaze Testing, Enameling, Ceramics, Metal Melting, Glass Fusing.
Innovative technologies, like Tabletop’s RAPIDHEAT system, which uses high temperature thermocouples to manage and distribute heat efficiently, provide the ability to build a metal clay kiln which quickly heats up to 2200 F (1205 C). At 100% heating times of less than 10 minutes, our RapidFire Pro series kilns will help to manage both time and costs, ensuring you can focus on what you do best!
Description
![]() | ![]() |
- Outside Dimensions: 8″ x 7″ x 13″ (W x D x H)
- Firing Chamber Dimensions: 6″ x 5″ x 6″ (W x D x H)
- Product Weight: 12 Lbs
- Max Heating Temp: 2200 F (1205 C)
- Power: 1500 W with standard 15 Amp circuit
- Coiled Type Resistance Wire
- Controller Type: Digital