Assaying for Copper

Procedure Residual Copper Soluble Analysis -Assay Method -Acid

METHOD for SEQUENTIAL AND RESIDUAL COPPER ANALYSIS PURPOSE:    To determine, through sequential dissolution, the probable copper distribution by copper mineral in a sample. SCOPE: Matrix: Copper ores   Analyte: Copper (Cu)   Range: <1-20%. Accuracy/Precision:    This method is not intended to be accurate since there is not one standard procedure for the determination of non-sulphide copper.  … Read more