What pH do I separate Chalcopyrite Galena Sphalerite by Flotation

pH Ranges for Sequential Cu Pb Zn Flotation | Separation

Sequential Cu Pb Zn Flotation Separation

To understand froth flotation, first read that article and come back to read about sequential flotation of Copper, Lead and Zinc. Given a baseline amount of frother and collector, these curves are the approximate/relative rate of flotation recovery of Copper (Chalcopyrite/Bornite/Chalcocite/Covellite/Tennantite/Enargite/Tetrahedrite /Freibergite ), Lead (Galena) and Zinc (Sphalerite) as well as iron (pyrite/arsenopyrite) minerals VS … Read more