The 150mm (6″) elbows have a S value of 1.7 per Table II. This multiplied by 10 and 6″(150 mm) gives an equivalent length of straight pipe of 102′(31m).
The 150mm (6″) elbows have a S value of 1.7 per Table II. This multiplied by 10 and 6″(150 mm) gives an equivalent length of straight pipe of 102′(31m).