The 911MPEPPGR426 is a small 300 kilo to 3.5 ton per 24 hour day capacity grinding mill acting primarily as a rod mill but can effortlessly be converted to a ball mill. Thanks to the integrated spiral classifier, it forms an easy to operate closed-circuit grinding plant. It includes a fine ore hopper, vibrating feeder and starter rod load.
It is the perfect small grinding circuit for pilot plant operations or small micro mining. Under specific conditions, it will grind finely crushed ( -6mm) ore to 75 microns. This is a Dual Media mill (rod or ball).
This continuous grinding mill is offered as a rod mill or ball mill of 420 mm X 600 mm (17″ X 24″) or as a grate discharge ball mill of 420 mm X 450 mm (17″ X 18″).
Motors 220V and 440V.