chromite fines flotation (1 reply)

G
Gomolemo Thembo
5 months ago
Gomolemo Thembo 5 months ago

Which collector is the best for floating the chromite fines from the tailings dam?

SmartDog
5 months ago
SmartDog 5 months ago

Generally either fatty acids or akrylomides are used for chromite, BUT... the actually selection is dependent on water chemistry,  mineralization of the chromite, other mineral specieces present, and what previous processes were used.  Only way to REALLY know is by laboratory testing and then pilot plant tests.  