Low pulp density PGM Flotation (1 reply)

R
rgov1992
11 months ago
rgov1992 11 months ago

Hi all,

 

I would like some advice on how to improve froth stability and pgm flotation performance at low pulp densities of about 10% solids.

Thanks

David
11 months ago
David 11 months ago

what frother are you using?