Froth Flotation (Sulphide & Oxide)

Froth Flotation (Sulphide & Oxide)2017-04-04T06:57:31-04:00
  • To participate in the 911Metallurgist Forums, be sure to JOINLOGIN
  • Use Add New Topic to ask a New Question/Discussion about Flotation.
  • OR Select a Topic that Interests you.
  • Use Add Reply = to Reply/Participate in a Topic/Discussion (most frequent).
    Using Add Reply allows you to Attach Images or PDF files and provide a more complete input.
  • Use Add Comment = to comment on someone else’s Reply in an already active Topic/Discussion.

Upgrading of low grade carbonaceous phosphate (2 replies and 1 comment)

Fati
3 years ago
Fati 3 years ago

Could you please suggest me some depressants that depress only carbonate and not apatite minerals

BAUD
3 years ago
BAUD 3 years ago

Please, can you share with the group:
- the mineral composition of your ore;
- the liberation size;
- the current flotation conditions;
- the mineral composition of the concentrate and the recovery.

 

Marshal Meru
3 years ago
Marshal Meru 3 years ago

read this also.

Fati
3 years ago

Thank you Marshal Meru for your answer, it's an interesting article... but I'm looking for carbonate depressants because I'm planning to direct float apatite while depressing carbonate minerals.

Please join and login to participate and leave a comment.

BUY Laboratory & Small Plant Process Equipment

We have all the laboratory and plant equipment you need to test or build/operate your plant.

ENTER our Mining Equipment' Store

We Sell EQUIPMENT for all types of Mineral Treatment PROCESSES and Laboratory Testing needs

Do you need METALLURGICAL TESTING of your ORE?

View the Services we Provide

911Metallurgist Mineral Processing & Process Development Laboratory

We have a metallurgical test for every possible mineral type and treatment.

Need ENGINEERING Services or Plant TROUBLESHOOTING?

We can IMPROVE ALL PLANTS / Mineral Processing Engineering & LABORATORY Ore Testing

911Metallurgy Engineering

Contact us for process engineering, metallurgical investigations, plant optimization, plant troubleshooting, needs. WE “FIX” METALLURGY.

I Need Consulting Engineering Help
I Need Ore Laboratory Testing