Adjustable Thermo-Electric Pyrometer

Frequently in using a thermo-electric pyrometer for measuring the temperature of a furnace, a hole is drilled at the back or side of the furnace, through which is introduced the tube containing the thermocouple. At times the couple is left almost where it drops, for the reason that it soon becomes too hot to be […]