Acid Activated Clay Adsorption Properties
Acid Treatment of Bentonite: Under the influence of a mineral acid the exchangeable alkaline earth ions of bentonite are substituted by hydrogen ions. Moreover, depending on the acid concentration, temperature, pressure and reaction time, a more or less pronounced leaching process takes place. Thereby Al-, Fe- and Mg-ions are extracted from the octahedron layers. This results … Read more