How to Remove Arsenic, Antimony & Bismuth from Copper

The ores of copper are usually associated with minerals containing arsenic, antimony and bismuth. Whatever the means adopted for extracting the copper, these metals are usually found, to a greater or less extent, in the product. There is, however, usually some elimination in the various metallurgical operations to which the ores are subjected, and some … Read more