Percent Solids to Specific Gravity Conversion of Slurry

calculate slurry SG

Here is the formula for specific gravity of a slurry, S is: S = specific gravity of slurry Si= specific gravity of liquid phase Ss= specific gravity of solids phase Cw = concentration of solids by weight Cv= concentration of solids by volume EXAMPLE: if the liquid has a specific gravity of 1.2 and the concentration […]