Arsenic Removal from Water
The removal of arsenic from water has been practiced for many years (8-11) but with the recent emphasis on clean water standards there has been renewed activity in relation to the problem. The methods which have been investigated include precipitation, co-precipitation, adsorption, ion exchange and liquid-liquid extraction but to date only precipitation and co-precipitation processes … Read more