The gold mining industry in Tanzania is looking to make a revolution with the help of the initiative Fairtrade International. The idea was recently announced and is going to impact 12 mines in Tanzania, Uganda and Kenya, creating the first batch of African ethical gold within a year. The goal is to put an end […]

Metallurgical Accounting Formulas

Two product formula

Have you been looking for a quick way how to calculate your flotation circuit’s metal recovery?  You have no concentrate weights all you have are metal assays.  Here are the assay based recovery formulas you can use for your metallurgical accounting.  Using these formulas, the Metallurgical/Metallurgy performance of the concentration plant or of a particular mill […]

SAG Mill Ball Size Evaluator | Evaluation Factors | Calculate Diameter

Are My Balls Big Enough

Lets calculate/select/pick a new ball for your SAG mill.  Now, lets suppose you have a SAG Mill and Ball Mill that are not drawing full kW Power.  The SAG Mill has a “small” circulation load of oversize given be the 3/8″ trommel screen and the 1/2″ x 1 1/4″ discharge grates.  The load of 4″ balls […]

Mining technology firm creates new system to process platinum

00151681 b094defe4837b1eee14b6f2a65ca187a arc614x376 w614 us1

The mineral processing plant manufacturer Appropriate Process Technologies (APT) is currently changing its strategy to target platinum miners, in Zimbabwe. The company is designing a new modular platinum gravity recovery system that can be used to process primary ores. The firm’s chief executive, Kevin Peacocke, said in a statement that: We are focusing more on designing and incorporating […]

Calculate Recoveries with 2 or 3 Product Formulas

Two Product Recovery Formula

Here is the formula you need to calculate Metal Recoveries using Assays only.  You have two products/concentrates.  This will save you time in your metallurgy accounting calculations.  Some call the same formula the two (2) product other the three (3) product formula. Frequently, a concentrator will mill a complex ore requiring the production of two separate […]

Mineral Processing Calculators

A Metallurgist needs certain toll mineral processing calculators or tools. 911Metallurgist Calculators Calculate the Flotation Cell & Conditioner Capacities/Volume Need in a Circuit S.G. Math & Conversion Calculate the Specific Gravity or Ores and Rocks How to convert a Pulp Density (%Solids) to SG Specific Gravity Circulating Loads How to Calculate a Grinding Circuit’s Circulating Load […]

Flotation Reagent Metering Pumps

Flotation Reagent Metering Pumps

I recently did a reagent plant trial and worked with a pretty nice flotation reagent metering pumps.  The pump is supplied by https://www.pmps.co.za This portable reagent supply unit is a mechanical diaphragm metering pump.  As see on https://www.pmps.co.za/obl-mechanical-diaphragm-dosing-pump They even had “Water Driven Pumps” Other pumps I never worked with include https://www.awe-ltd.co.uk/products/dosing_pumps_electronic.html and https://www.lutzjescoamerica.com/index.php?id=1645   Also https://www.911metallurgist.com/mibc-frother-pump

10 Insane Russian mines

Kuznetsk opencast coal mine mod

Russia’s size and geographic conditions lead to the existence of many amazing mineral deposits that make the nation a hub for mining activities. Some of the world’s most incredible mines are located in this wonderful country. 1. Yakutia Mir Mine The world’s biggest diamond mine is located in Eastern Siberia, Russia. The Mir mine is 1,722 ft deep, being the […]

Do I Need Bigger and Larger SAG Mill Balls

SAG Balls

How do you know if a larger SAG ball will increase your tonnage and how to select it?  When is it time to change to a larger Ball in your SAG Mill? It’s difficult to generalize on SAG mill ball size selection as it depends on a number of factors: Ore properties Level of impact […]