Electrowinning Mercury in Gold Pregnant Solution
Many gold-bearing ores in the Western United States also contain small amounts of mercury. The presence of mercury creates potential pollution and health hazards during
Many gold-bearing ores in the Western United States also contain small amounts of mercury. The presence of mercury creates potential pollution and health hazards during
Effective recycling or disposal of flue dusts is a continuing problem, particularly for secondary smelters treating low-grade Cu scrap. The Bureau of Mines investigated a
The Bureau of Mines conducted column-leaching tests on 25 domestic Mn ores to determine the feasibility of extracting Mn by in situ or heap leaching
We studied the problem of corundum formation on refractory linings in aluminum recycling furnaces. A laboratory test was developed for evaluating refractories in contact with
Research was conducted by the Bureau of Mines to determine the feasibility of using electrokinetic densification to dewater Bayer process red mud, magnetic black mud
The effect of fluoride inclusions on the properties of titanium produced from the Bureau of Mines developed induction slag melting process is of concern to
Ore grinding is a major cost operation for the mineral processing industry. The U.S. mining industry consumes more than 400,000 st of grinding rods, balls,
The Bureau of Mines surveyed waste disposal sites at 18 metal and non-metal mines and conducted laboratory and full-scale field tests to determine the effects
A mathematical modeling method was developed by the Bureau of Mines for the prediction of the principal equilibrium species in the solvent extraction of copper.
As part of its research program on column flotation, we performed studies on (1) column flotation amenability and comparison with conventional flotation results for over