Several preliminary tests were conducted as a function of drum type (standard, interpole, etc.) and feed temperature. The results from these tests indicate that the
Several preliminary tests were conducted as a function of drum type (standard, interpole, etc.) and feed temperature. The results from these tests indicate that the
Pulsed columns, like other pulsed columns, consist of an active column section with decanters on either end. Test columns are usually in the 40 mm
Interests in the hydrometallurgical processing of primary sulfide concentrates have revived because leaching in chloride media is rapid and is capable of recovering sulfur in
Strain relief measurement techniques were used to quantify stress in the underground pillar and to compare stress relief to seismic and ultrasonic core velocities. These
Three mills are now operated by the Consolidated Mining & Smelting Co. of Canada, Ltd.: (1) The Sullivan Concentrator, Chapman Camp, B. C. (near Kimberley,
It is also fairly well-known, that it is by far much more difficult to achieve high efficiency with dry classifying than with wet. Hence, it
The principle of the sample flows of the analyzer system is shown in Figure 4. As the analyzers are located in a separate room, many
Alternative reagents for gold leaching include thiocyanate (SCN-) and thiourea (SC(NH2)2). They are considered less toxic and more environmentally acceptable when compared to cyanide. One
After filling the column with water, the teeter water flow rate was set to produce the desired cut size. The feed water was adjusted to
Curved pulp lifters have been incorporated in SAG and AG mills in Australia. The aims have been to ensure complete discharge, at high throughput, of