Fine Coal Recovery

Fine Coal Recovery and Mine Backfill Preparation: The coal mines in the Sunnyside, Utah, area have been mined continuously since 1896 and prospered as Bee Hive

Read More »
Concentrator Manuals/Procedures

Mine Backfill Plant

Backfill Preparation Plant: Mine roof support problems were a major concern that necessitated the use of backfill to supplement conventional means of support. Roof supports account

Read More »
grinding-flotation-counter-current
Various

Designing Small CCD Cyanide Plant

The world demand for gold and international economic pressures for an advance in price have accelerated interest in gold and silver production. Many opportunities exist

Read More »

SILVER LEAD ZINC FLOTATION

The recovery of silver minerals occurring in a lead- zinc sulfide ore is efficiently accomplished using the above flowsheet. The process consists of selective flotation

Read More »

Laboratory Gas Generators

There are many forms of these, and to describe them would of itself fill a volume. A simple generator for hydrogen sulphide, carbon dioxide or

Read More »

Laboratory U-tubes

Gases, Drying and Absorbing.—For this purpose U-tubes, potash bulbs, calcium chloride tubes and calcium chloride jars are used. U-tubes, Fig. 103, are made in a

Read More »