Percent Solids to Specific Gravity Conversion of Slurry
Here is the formula for specific gravity of a slurry, S is: S = specific gravity of slurry Si= specific gravity of liquid phase Ss= specific

Here is the formula for specific gravity of a slurry, S is: S = specific gravity of slurry Si= specific gravity of liquid phase Ss= specific

Part of your slurry dewatering system is the production of a filter cake. Obviously that cake must have as low a moisture as possible. A

How to Size a Cyclone or Hydrocyclone has a well establish step-by-step process for which Richard A. Arterburn was a pioneer. Since this paper and its

Let me point you to two good papers on the flotation of mixed copper oxide and sulphide minerals with xanthate and hydroxamate collectors. A great detailed

What is the Bond Work Index Formula-Equation? In case you had forgotten, here is a classic: You can read all the details of this now “Biblical”

Learning how to compare flotation test results made easy: One set of test from Lab A is displayed by the red dots and compare to

An on-stream analyzer and small regrind cyclones (their small 1/2″ Apexes) were being plugged by trash coming from the underground mine in the form of

Use the conversion factors in this Table which uses Stoichiometry to approximately convert metal assays to minerals. If you know your sample has only Chalcopyrite as a

A good grinding circuit survey (and flotation circuit sampling) is only as good as the sample cutter used for each slurry stream. Correct sampler volume

A Schuhmann Plot help smooth out particle size data. I attach a graph created for a settling test of flotation concentrates. You draw/create a Schuhmann Plot