automatic grind control grinding circuit
Grinding

Automatic Grinding Mill Control

There are presently in use many grinding mill control schemes and concepts. In this case, one operating method of controlling the particle size of the

Read More »
flotation influence of percent solids
Assaying

Gangue Assay

On-stream analysis is a much more rapid means of obtaining true assays of a flowing product when compared to wet chemistry or “grab” samples dried,

Read More »
sulfide-ion-leaching eletron micrograph
Hydrometallurgy

Sulfide Ion Leaching Kinetic of Wulfenite

The principle oxide minerals of molybdenum are wulfenite (PbMoO4), ferrimolybdite (Fe2(MoO4)3·nH2O), powellite (CaMoO4), and ilsemannite (Mo3O4). Wulfenite is found in Arizona, New Mexico, Nevada, Utah,

Read More »
waste-dumps test strip circuit
Mining

High Waste Dump Stability

The height, structure, rapid rate of growth, and anticipated leaching suggested the possibility of dump failure. In order to evaluate this possibility, an outside consulting

Read More »
reagent concentrator
Reagents & Chemicals

Flotation Reagent Manufacturing

Manufacture and mixing of flotation reagents at the mill site provides an economic and convenient method of maintaining a continuous and fresh supply of reagents

Read More »