Jigging Separation Process Principle
The Mineral Jig is not just another gravity Separation Process. It is a highly efficient selective pulsator and concentrating machine which has the ability to treat an unclassified feed separating solids having only a slight differential in settling rates, with only a minimum addition of water. 1000s of these Mineral Jigging machines are now in operation on … Read more