Fine Gold Recovery Equipment

Showing all 3 results
  • fine gold recovery equipment (1)falcon concentrator fine gold recovery equipment
    fine gold recovery equipment (1) falcon concentrator fine gold recovery equipment
    The i150 Gravity Concentrator is the smallest of the World famous iCONs. This is a gravimetric concentrator that uses enhanced gravity (G’s) to concentrate the 'free’ heavy minerals. It is also known as a centrifugal concentrator because of the centrifugal actcanada manufacturerion of the spinning bowl. The process uses only water and an electric motor to concentrate the precious heavy minerals from a slurry. The i150 is the heart of the iCON product line. At a capacity of 2 tons per hour solids, the iCON i150 is commonly used for:
    • Hard Rock Precious Mineral Recovery - due to the 2 TPH capacity
    • Exploration/Sampling - due to the convenient size/mobility
    • Artisanal Placer mining - due to it economic low- price and high reliability
    • Recovering fine gold down to 400 mesh (37 microns)
    Why is the i150 "Mini Falcon" the best gold centrifugal concentrator:
    • Low Machine Weight
    • distributor supplier manufacturerOnly 1 Moving Part
    • Wear Components Replaceable in the Field
    • Serviceable with Common Hand Tools
    • Ease of Installation/Operation
    • Excellent Value at a Fair Price
    • 1.5 minute Clean Out Time
    • High Concentration Ratios
    • VFD / Soft Start Included
    If you are not sure your gold can be recovered by gravity; contact us, we'll tell you.
  • laboratory gravity concentratorlaboratory_gravity_concentrator
    laboratory gravity concentrator laboratory_gravity_concentrator
    The Falcon L40 enhanced gravity concentrator has a bowl diameter of 4” and is specifically designed for laboratory test-work on small ore samples. Applications include the concentration and upgrading of gold, platinum group metals, mineral sands, chromite, tin, tantalum, tungsten, iron ore, cobalt as well as many other metals and minerals with sufficient differences in specific gravity. It is used for the simulation of industrial scale Falcon high-G gold centrifuge models: Ultra-Fine (UF), Semi-Batch (SB), Continuous (C). The applicable model and operating parameters are dependent on sample specific features, such as the particle size and desired mass yield.canada manufacturer A fabricated adjustable L40 steel stand and 50 liter agitated stainless steel tank are optional additions. The machine is of stainless steel construction and a two stage UHMW polyethylene bowl. The materials of construction have been carefully selected to minimize the possibility for contamination between samples. The rugged functional design of this unit means that it is perfect for use at an exploration site or mineral processing laboratory.
  • flour gold recovery equipmentfine gold recovery equipment (24) Sale!
    flour gold recovery equipment fine gold recovery equipment (24)
    The i350 is a family member of the Falcon Gravity Concentrators Gold Mining Equipment which has revolutionizing the world of alluvial gold mining and dredging the same way its little brother, the i150, has impacted the world of hard rock mining. This is a gravimetric mineral concentrator that uses enhanced gravity (G’s) to concentrate the ‘free’ heavy minerals. It is also known as a centrifugal concentrator because of the centrifugal action of the spinning bowl. This equipment lets you Recover Gold without Chemicals with a process that uses only water and an electric motor to concentrate the precious heavy minerals from a slurry.canada manufacturer At a capacity of 10-15 tons per hour solids, the i350 is commonly used for:
    • Alluvial / Placer Mining
    • Dredging
    • Hardrock mining within a grinding circuit
    Due to the ability to capture fine gold and the high concentration ratios, the i350 Gravity Concentrator can be used to minimize the length of your sluice and minimize the amount of concentrate in your operation. If you host GRG Gravity Recoverable Gold, the i350 is the ultimate gold recovery machine.

Likely the Best Fine Gold Recovery Equipment based on the enhanced centrifugal forces, like the Falcon Concentrator, has a maximum capacity of 150 t/h. The concentrator has proven effective in various minerals sectors link gold, Cu, Sn, Coal, Iron ore, Ag, Heavy mineral and most significantly tantalum where Falcon has achieved excellent results.

fine gold recovery equipment the best fine gold recovery system

Schematic diagram of a Falcon continuous concentrator

ADVANCED GRAVITY TECHNIQUES

Gravity concentration technique is the most simple and economical of all methods of concentration applied in mineral processing. It permits the recovery of values at coarse a size range as possible. The separation of mineral particles are generally based by exploiting the difference in density between the two minerals. At present, the gravity concentration technique is widely used for the treatment of various traditional raw materials. Tin. tungsten, chromite, iron ore, coal as well as the heavy mineral of alluvial or beach sands etc. are commonly processed by this technique. Now days lot of new and advanced equipments have been developed to separated the finely divided minerals from the gangue materials. Some of them arc reviewed here.

The Falcon Concentrator is a Fine Gold Recovery Equipment made of a rotating bowl with the smooth inclined wall. The feed slurry enters the bottom of the bowl and gets stratified along the bowl wall. The heavier material settles on the wall while the lighter particles are pushed to the lip of the bowl and discharged as the overflow. The heavier fraction settled on the bowl wall is continuously removed through a nozzle located at the top of the bowl.

Gravity concentration is the oldest beneficiation technique adopted by the mankind. Gravity concentration is simple, cheap and efficient to treat coarse high-grade ores. However the low-grade ores need to be reduced to fine sizes for better liberation and traditional gravity concentration techniques are not capable of treating fines. After the invention of froth flotation in the beginning of 20th century, gravity concentration was pushed to the back seat. But the gravity concentration made a comeback by the end of 20th century due to:

  • Availability of new advanced techniques capable of treating fines, ultra-fines and Fine Gold Recovery.
  • Rising costs of reagents for flotation operation.
  • Environmental concerns related to the flotation process.

The advanced gravity concentration techniques essentially use centrifugal force to provide enhanced gravity to efficiently treat fines. Some of the successful Enhanced Gravity Concentration technologies and Fine Gold Recovery Equipment that found application in the mineral processing industry are Falcon Concentrator and Mozley Multi-Gravity Separator.

As a Fine Gold Recovery Equipment, the Falcon concentrators rely on a rotating bowl to generate high centrifugal accelerations similar to Knelson concentrators. The feed slurry rises upward over a slightly inclined smooth wall Stratification of higher-density particles occurs toward the bowl wall, and lower-density particles move toward the center of the bowl. Different models vary in the way they collect and produce the concentrate

In the semi-batch Fine Gold Recovery Unit, the upgraded product that has been forced against the bowl wall is made to move into a vertical, fluidized collection zone in the upper portion of the bowl. The collection zone consists of a number of rings that have pressurized water injected from the back, effectively elutriating and cleaning the concentrate that sits in these collection rings until a rinse cycle begins. These machines are known as semi-batch devices because they continually accept feed during the run cycle but only produce concentrate during periodic rinse cycles. Run times range from 30 minutes to several hours depending on the application, while the rinse times are generally less than a minute. The throughput rates range from 1 to 400 t/h The centrifugal accelerations range from 50 to 200 G These units are mainly used in precious metal recovery plants.

In continuous devices, at the top of the bowl is a ring of specially designed concentrate flow hoppers, followed by pneumatically controlled variable orifice valves. These valves allow for a constant stream of concentrate to be produced. The continuous Fine Gold Recovery concentrator is able to vary mass pull to concentrate by adjusting valve orifice size through changes in air pressure. Because of their high mass pull rates of 5% to 40%, these units are used in the recovery’ and upgrade of tin, tantalum, tungsten, chrome, cobalt, iron, fine oxidized coal, and uranium ores. The ultrafine units are designed to concentrate material below 50 um at less than 20% solids and may be typically used in deslime cyclone overflow streams.

The Falcon concentrator is another spinning batch Fine Gold Recovery Equipment designed principally for the recovery of free gold in grinding circuit classifier underflows where, again, a very small (<1%) mass pull to concentrate is required. The feed first flows up the sides of a cone-shaped bowl, where it stratifies according to particle density before passing over a concentrate bed fluidized from behind by back-pressure (process) water. The bed retains dense particles such as gold, and lighter gangue particles are washed over the top. Periodically the feed is stopped, the bed rinsed to remove any remaining lights and is then flushed out as the heavy product. Rinsing/flushing frequency, which is under automatic control, is determined from grade and recovery requirements.

The units come in several designs, the Semi-Batch (SB), Ultrafine (UF), and i-Con. designed for small scale and artisanal miners.

These batch centrifugal concentrators have been widely applied in the recovery of Fine Gold, platinum, silver, mercury, and native copper.

best fine gold recovery system best fine gold recovery system
best fine gold recovery system falcon fine gold gravity concentrator (1)
falcon fine gold gravity concentrator (6) best fine gold recovery system