dewatering of talc slurry laboratory flocculation
Thickening

Dewatering Talc Slurry

Table of ContentsDescription of Samples TestedLaboratory Batch Dewatering Tests of Talc SlurryInitial Testing of FlocculantsDewatering of Talc Slurry with Hercofloc 1027Continuous Dewatering Tests of Talc

Read More »
sedimentation pond design typical
Mining

Sedimentation Pond Design

Table of ContentsSedimentation Pond Design CriteriaSedimentation Pond Design ProceduresError Analysis In the preliminary phases of mine planning it is often desirable to quickly estimate approximate

Read More »
screen units crusher
Classification

Large Screen Unit Design

The trend in new process plant design is moving towards the multi-screened large capacity modular design. As a result, multiplicity of process equipment will be

Read More »
derrick-multifeed screen dense medium circuit
Classification

Derrick Screens

General widespread interest in fine coal cleaning circuits did not occur in the United States until the mid 1960’s. Up until this period the relatively

Read More »
copper-moly separation flotation feed
Flotation

Copper Moly Separation Depressant Roles

Table of ContentsExperimentalResults and DiscussionSummary and Conclusions Bulk and differential laboratory flotation tests have been carried out using a synthetic mixture of chalcopyrite and molybdenum

Read More »
crushed-pellets improvement of crushing system
Steel

Crushed Pellets

Table of ContentsBlast furnace operation test using crushed pelletsResults of blast furnace operation test with crushed pellets At the Kakogawa works of Kobe Steel. Ltd.,

Read More »
concrete crib design demonstrations actual layout
Mining

Concrete Crib Design

Table of ContentsDemonstrations at Sunnyside Mine No. 1Advancing Tailgate of 10 Left Longwall PanelDouble-Entry Tailgate of 17 Left Longwall PanelDemonstrations at the York Canyon Mine