cyanide-leaching pachuca leaching vessel for mercury extraction
Electrometallurgy

Precipitation of Mercury in Cyanide Gold Leaching

Table of ContentsMaterial Equipment and Operating ProcedureResults and DiscussionEffect of Process Variables on Mercury ExtractionCyanide ConcentrationLeaching TimeSolution pHTemperatureParticle SizeMercury Removal by Sulfide PrecipitationMercury Precipitation from

Read More »
potash recovery process research unit
Blog

Potash Recovery by Solar Evaporation & Flotation

Table of ContentsLaboratory-Scale ResearchEvaporation ExperimentsDescription of Process and Waste BrinesLaboratory Evaporation ProcedureEvaporation Results and DiscussionBeneficiation of Crude EvaporitesGrinding StudiesFlotation of Chloride EvaporitesFlotation of Sulfate-Chloride EvaporitesHigh-Sulfate

Read More »
oxygen self-rescuers cse au-9al
Blog

Oxygen Self Rescuers

Table of ContentsDescription of an Oxygen Self RescuerNiosh-ApprovedCSE AU-9AlDraeger OXY-SR 60BMSA 60-Min SCSROcenco EBA 6.5PASS 700U.S.D. SCEBA-60ForeignAuer SSR-90AZG-40Draeger OXY-SR 30Draeger OXY-SR 45Fenzy Spiral IIWC-7Bureau Of Mines-Developed

Read More »
on-stream analysis excitation
Assaying

On Stream Analysis

Table of ContentsRadiometric TechniquesX-Ray Tube TechniquesNeutron ActivationA Comparison Between Radiometric and X-Ray Tube Techniques An on-stream analyser cannot be considered in isolation from the mineral

Read More »
carnallite-ore flotation unit
Flotation

How to Recover Potash from Carnallite

Table of ContentsSample DescriptionContinuous Flotation Unit Design and OperationDesign For Insoluble-Slimes FlotationDesign For Direct FlotationOperationSampling and Data AnalysisExperimental ResultsMaterial Balance and Economic EvaluationSummary and ConclusionsAppendix—Economic EvaluationCapital

Read More »
platinum-group-metal cell for electrolytic addition
Electrometallurgy

Electro-depositing PGM Platinum Group Metal Coatings

Table of ContentsHistorical PerspectiveScope of ReportElectrolyte PreparationDrying and Fusing of SaltsPlatinum-Group Metal AdditionRole of OxygenElectrodepositionSubstrate Surface PreparationMolybdenum-Base AlloysIron-Base AlloysElectroplatingPlatinumRhodiumPlatinum-Rhodium AlloysPalladiumIridium and RutheniumSubstrate EffectsIncomplete PreparationMicrostructureSummary The

Read More »
gold-uranium-pregnant-solution fluidised blanket clarifier
Hydrometallurgy

Gold & Uranium Pregnant Solution Clarification

Table of ContentsExperimentalFiltrationDiscussion of ResultsFiltrationPregnant Solution Clarification Before precipitation of gold can be commenced the relatively high suspended solids content (on average 350 mg/L) of