A stock of 300 pounds of 1 5/8-inch sillimanite balls was donated by the Champion Spark Plug Co. for grinding tests. They were true spheres,

Read More »

Effect of Pulp Density on Grinding

Table of ContentsBatch Mill Grinding of OreOpen Circuit Grinding Batch Mill Grinding of Ore Batch grinding affords the best opportunity for first studies of pulp consistency. Table

Read More »

Ball Mills vs Rod Mills

Table of ContentsSelective and Non-Selective GrindingLarge Balls & Small Rods Compared When the mill is rotated without feed or with very fine feed, the rods

Read More »

Batch Ball Mill Grinding

Table of ContentsDry-Batch Ball Milling with Various Ore ChargesDry-Batch Ball Milling with Equal Ore Charges and at Various Speeds Chert, which is very hard, and

Read More »