Low Angle Slurry Pot Test

Table of ContentsSlurry Pot Equipment and SpecimensSlurry Pot ProcedureSlurry Pot Results Transporting minerals as a slurry is an efficient means of transportation and is done

Read More »

Dry-Particle Erosive Wear Test

Table of ContentsDry-Particle Equipment and SpecimenDry-Particle ProcedureDry-Particle Typical Results Dry-particle erosive wear can be classified as low-stress, two-body wear, the same type as in the

Read More »

Taber Abraser Test

Table of ContentsTaber Abraser Equipment and SpecimensTaber Abraser ProcedureAbrasion Resistance Test of Refractory Materials The Taber Abraser is a commercial wear tester designed to test

Read More »

DSRW Abrasive Wear Test

Table of ContentsDSRW Equipment and SpecimenDSRW ProcedureDSRW Results and Discussion The dry-sand, rubber-wheel (DSRW) abrasion test apparatus simulates low-stress, three-body abrasive wear. This type of

Read More »

Wear Testing Laboratory

Table of ContentsDescription of Tests and EquipmentAbrasive Wear The laboratory wear testing capabilities are described. Wear tests are used to support the group’s research efforts

Read More »

Potash Feldspar Recovery Process

Table of ContentsDescription of SamplesLaboratory Batch Flotation TestsThe Citric Acid-Sodium Carbonate-Fatty Acid MethodThe Sulfuric Acid-Petroleum Sulfonate MethodThe Hydrofluoric Acid-Dixanthogen MethodVariation of the Citric Acid-Sodium Carbonate-

Read More »

How to Reduce Pumping Cost

The prime objective of this paper is to call attention to possibilities of reducing the cost of pumping, generally by reducing inflow into the mine

Read More »

Make Alumina using Hydrochloric Acid

Table of ContentsMaterials, Equipment, and ProceduresLeachingFiltering and WashingEvaporation to 25 Wt-Pct AlCl3OxidationSolvent ExtractionReaction of Iron Strip Solution with ClayEvaporation to 30 Wt-Pct AlCl3Sparging With HCl

Read More »

Platinum – Palladium Flotation

Table of ContentsGeneral Geology and MineralogyFlotation Test Equipment & ProcedurePreliminary Flotation TestsOptimization of Rougher Flotationwith Mercaptobenzothiazole Collector and Sulfuric Acid ModifierEffect of Recycling Water in

Read More »