Flocculation Dewatering Clay

Table of ContentsDescription of Samples TestedInitial Testing of Reagents for FlocculationBench-Scale Batch Flocculation TestsTest ProcedureEffectiveness of Polyethylene Oxide PolymersSEM Examination of Flocculated SystemsTests on Plant

Read More »

Aluminum Sulfate Leach Solution Extracting Iron

Table of ContentsMaterialsEquipment and ProcedureResults and DiscussionDetermining Leaching ConditionsDetermining Extraction ConditionsDetermining Stripping ConditionsMultistage StudiesDetermining Alumina PurityConclusions Increasing usage of aluminum and competition for foreign reserves

Read More »
diamond processing plant & equipment
Flowsheets & Flowcharts

Diamond Processing Plant & Equipment

World demand and production of diamonds both for gem and industrial purposes has increased nearly five-fold during the past 25 years. Improved mining and recovery

Read More »
grinding-flotation-horsepower
Flotation

COARSE FLOTATION

COARSE FLOTATION OFFERS IMPORTANT SAVINGS THROUGH REDUCED OPERATING COSTS Grinding cost varies greatly depending upon the size reduction required. For example, it takes approximately 50%

Read More »
placer deposit processing
Flowsheets & Flowcharts

Placer Deposit Processing

The handling of large quantities of gold-bearing gravels is of utmost importance for most successful placer operations. In addition to providing efficient washing and recovery

Read More »
grinding-flotation-chute
Equipment

CHUTE SAMPLER

CHUTE SAMPLER FINDS WIDE APPLICATION ON DRY MATERIALS Many installations are confronted with sampler arrangements where the material is handled in chutes and installation of

Read More »

Zinc Electrolysis

Table of ContentsZinc Chloride-Alkali Metal Chloride ElectrolytesProcedure & ResultsLiquidus Temperature DiagramsEffect of Electrolyte CompositionSludge Formation in ElectrolytesInternally Heated Electrolytic CellOperation of a 1,500-Amp CellConclusions Zinc

Read More »

Electroslag & Electric Arc Furnace Processes

Table of ContentsExperimentalMaterialsEquipmentMelting ProceduresIngot TestingResultsElectric-Arc-Furnace-Melted IngotsElectroslag-Remelted IngotsForged and Rolled BarMicrocleanness and MicroporosityMechanical PropertiesTensile PropertiesImpact PropertiesMicroscopyOpticalScanning Electron MicroscopyDiscussions and Conclusions Demand for pressure vessel steels for

Read More »

Electrorefining Copper

Table of ContentsApparatus and Experimental TechniquesRotating Electrode CellsSingle Channel CellsMulti-channel CellResultsRotating Electrode CellsRing ElectrodesCylinder ElectrodesSingle-Channel CellSynthetic Electrolyte TestsTankhouse Electrolyte TestsComparison with Industrial Refining CellsMultichannel CellInitial