Huntington Mill
The Huntington Roller Mill, here described as a type of the many good roller mills now in use, is best suited for the fine crushing

The Huntington Roller Mill, here described as a type of the many good roller mills now in use, is best suited for the fine crushing

An amalgamation pan consists of a circular cast-iron pan, provided on the inside with a renewable false bottom of cast-iron—constituting the lower grinding surface—and a

The stamp battery must be regarded from two different points of view, (a) as a crushing machine, (b) as an amalgamating machine, and it should

Minimizing losses of gold in amalgamation will result in optimum Gold Amalgamation Recovery which may be ranged under the following heads: Loss of free gold contained in

The appearance in the tailings of free gold, which is not especially finely divided, but, nevertheless, is not in a condition to be amalgamated, may

So far, no account has been taken of the loss of gold which is contained in pyrites, as it has been assumed that these are

In order to keep the plates in proper condition so that successful amalgamation may be maintained, they must be prepared carefully, and the closest watch

The solid amalgam, which is retained in the canvas or wash-leather filters, usually contains from 30 to 45 per cent, of gold and silver, according

The earliest machines used for the purpose seem to have been stone mortars, in which the gold quartz was crushed by stone-hammers, or by large

The stamp mill‘s battery evolved, no doubt, from the pestle and mortar was not introduced until a comparatively recent date. Beckmann states that mortars, mills,