electrostatic separation roll-type
Blog

Photoelectric Charging & Electrostatic Separation

Table of ContentsPhotoconductivity Versus Photoemission of ElectronsUltraviolet Light Absorption in AirPhotoemission Effects of Conductive MineralsPhotoemission from Dust-Size ParticlesCharge Required for Dust Separation Electrostatic separation is

Read More »
iron-ore-pellets laboratory kiln
Pyrometallurgy

Effect of Preheating Iron Ore Pellets

Table of ContentsRaw MaterialsProcedure and EquipmentPelletizingExperimental WorkEquipmentResultsOxidation of MagnetiteSinteringEffect of Preheating Upon MetallizationEffect of Preheating Upon Pellet Properties The production of pre-reduced iron ore pellets

Read More »
recovering-plastics electrodynamic separator-2
Recycling

Electrodynamic Separator

Table of ContentsSample TestedApparatus and Procedures Used Several years ago, the Bureau of Mines initiated a program to develop effective methods for reclaiming and recycling

Read More »

Applied Mining Geology

The geologic notes are taken as soon as possible after the ground is broken so that any mistake in the mining may be corrected at

Read More »
raw urban refuse separation flowsheet
Recycling

Small Scale Metal Recycling Plant & Equipment

Table of ContentsTechnical ConsiderationsFlowsheetPilot Plant PerformanceProduct UtilizationProcess EconomicsFuture Plans Of the 220 million tons of refuse collected annually in the United States, it is estimated

Read More »
pyrite dry separation method cross section of centrifugal separator
Gravity Concentration

How to Remove Pyrite from Coal

Table of ContentsDry-Separation ProcessCentrifugal SeparationElectrostatic SeparationGrindability of Pyrite and Coal-An Aid in SeparationCombined Centrifugal-Electrostatic Separation In recent years, coal research has been directed toward environmental

Read More »
separating copper electric components
Smelting - Melting - Refining

How to Separate Copper from Scrap by Melting

Table of ContentsAcknowledgmentsLaboratory EvaluationExperimental ProcedureSweating With Other Predip TreatmentsElectronic Component SweatingDiscussion and Concluding RemarksCost EstimateDescription of ProcessesEstimating MethodCapital CostsOperating CostsEvaluation, Results, Discussion, and Conclusions The

Read More »
smelting of copper furnace
Pyrometallurgy

Copper Smelting

Table of ContentsCopper Smelting ProcessHeat Balance Using Pure Oxygen Versus AirCopper Smelting Furnace Construction and Refractories UsedTest Procedure and Discussion of ResultsSlag Composition, Losses, and

Read More »
samarium-cobalt permanent magnets microstructures
Equipment

Permanent Magnets

Table of ContentsAlloy PreparationPowder PreparationAlignment and CompactionSintering ProcedureMagnetic MeasurementsResults and DiscussionOptimum CompositionEffects of CompositionEffects of Sintering TemperatureEffects of Grinding The magnetic properties of rare earth-cobalt

Read More »