Mineral Processing Equations EQ

A Metallurgist or more correctly a Mineral Processing Engineer will often need to use these “common” Formulas & Equations for Process evaluation and calculations:   Circulating

Read More »
assaying arsenic
Laboratory Procedures

Arsenic Determination/Assaying

An assay method to measure arsenic using a MHS-10 and AA200 and Mercury Hydride System. Sample Preparation -Sample Weights to be used: Heads…………….. 0.3 g Cu Con……………..0.1

Read More »

Sodium Borohydride Make-up

Sodium Borohydride Solution Make-up Weigh 5 g of Sodium Borohydride and 2.5 g of KOH into a glass funnel inserted into 250 mL volumetric flask.

Read More »
factors_used_to_convert_metal_assays_to_mineral_assays
Laboratory Procedures

Gravimetric Factors

The factors used to convert metal assays to mineral assays in this MVT Mississippi Valley Type Deposits review is summarized below. The conversion factors are

Read More »