crushing drop-weight crusher assembly
Crushing & Screening

Laboratory Crushing Tests

Table of ContentsFracture of SolidsSize Distribution of Crushed MaterialEnergy Input Vs. New Surface Crushing has always been a major operation in the chemical and metallurgical

Read More »
sinter testing hydrogen reducibility apparatus
Steel

Sinter Testing

This report to the American iron and steel industry marks the completion of a 1949 survey of blast-furnace sinter practice sponsored by the Sub-committee on

Read More »

Zone Melting

Table of ContentsNormal FreezingZone-Leveling ProcessesZone-Refining ProcessesDiscussion If a charge of binary solid-solution alloy is melted and then frozen slowly from one end, as for example

Read More »
magnetic taconite piercing through rock
Mining

Jet-Piercing

Table of ContentsPiercing TechniqueJet-Piercing BlowpipePiercing Results During 1950 the jet-piercing process was used commercially in the piercing of primary blast-holes in magnetic taconite at the

Read More »
sponge iron plant anaconda
Steel

Sponge Iron

Sponge iron as produced at Anaconda is a fine, —35 mesh, impure product, about 50 pct metallic iron, obtained from the reduction of iron calcine

Read More »
dorrclone
Classification

DorrClone

Table of ContentsInstallationDorrClone Underflow ControlApplications and LimitationsDeslimingFlorida Pebble Rock PhosphateFine Size Classification This paper presents in a general manner some of the applications of the

Read More »
pipeline transportation phosphate line pumps
Pumping & Conveying

Pipeline Transportation of Phosphate

Table of ContentsPumping Florida Pebble MatrixPumping Tennessee MatrixHydraulic Transportation SystemTheoretical ConsiderationsPipeline LocationHydraulic Transportation System The pumping of solids in water suspension is an important part

Read More »